Mortar Smash Brick Guide

A field guide for people who can't walk past a good wall.

Mortar Smash is a free, plain-English guide to bricks: where they came from, the standard sizes in the UK, US, Germany and Australia, the main bond patterns (stretcher, English, Flemish and stack), how clay bricks are made, famous brick buildings, and how to care for and repoint brickwork. It also includes a brick and mortar calculator and an original arcade game, Mortar Smash.

A Short History of Bricks

People have been shaping mud into building blocks for roughly nine thousand years. The earliest known bricks, found in the Middle East, were simply sun-dried lumps of clay mixed with straw, pressed by hand and left to bake in the heat.

The big leap came with firing. Once builders discovered that clay heated in a kiln turned hard and water-resistant, bricks could survive rain and frost. Mesopotamian cities, the Indus Valley settlements and later the Romans all relied on fired brick, and Roman legions carried mobile kilns across their empire.

After a quieter period in parts of Europe, brick returned strongly in the Middle Ages, especially in regions short of good building stone such as the Low Countries and the Baltic coast. The Industrial Revolution brought steam-powered presses and continuous kilns, making bricks cheap enough to build whole cities of terraced houses, mills and railway viaducts.

Types & Sizes

Common brick

Everyday structural brick, usually hidden behind render or used in internal walls.

Facing brick

Made for looks: consistent colour, texture and sharp edges for the visible face of a wall.

Engineering brick

Dense, strong and low in water absorption. Ideal for foundations, sewers and retaining walls.

Firebrick

Refractory brick that withstands extreme heat, used to line fireplaces, kilns and furnaces.

Handmade & stock

Thrown into sanded moulds, giving creases and soft edges that look great in older houses.

Perforated & frogged

Holes or a hollow "frog" reduce weight and help the mortar key in.

StandardSize (L × W × H)
UK metric215 × 102.5 × 65 mm
US modular7⅝ × 3⅝ × 2¼ in
German NF240 × 115 × 71 mm
Australian230 × 110 × 76 mm

Sizes are designed so that with a 10 mm mortar joint, a brick's length equals two widths plus a joint, which is what makes bonding patterns work. Need a quantity for your own wall? Use our brick calculator for bricks per m², total bricks and mortar for each of these sizes, plus quick answers for common jobs like garden walls, piers and pillars, brick-on-edge coping and concrete for a garden wall footing. For cement and sand, try the mortar calculator. For which unit belongs on which job, including UK engineering Class A and B and US paving specifications, see which bricks for which jobs and frost resistance grades.

Bonds & Patterns

A "stretcher" shows its long side, a "header" shows its end. Bonds mix them so vertical joints never line up, spreading the load.

Stretcher bond — all stretchers, each course offset by half a brick. Common in modern cavity walls. See brick sizes for why the offsets work.
English bond — alternating courses of stretchers and headers. Very strong.
Flemish bond — headers and stretchers alternate within each course. Elegant and Georgian.
Stack bond — bricks stacked in a grid. Decorative only; needs reinforcement.

More detail, sources and a FAQ are in which brick bond suits which job.

How Bricks Are Made

  1. Winning the clay. Clay and shale are dug from quarries and left to weather.
  2. Preparation. The raw material is crushed, screened and mixed with water to a workable consistency.
  3. Shaping. Clay is either extruded as a long column and wire-cut, pressed into moulds, or thrown by hand.
  4. Drying. Green bricks are dried slowly over a day or more so they don't crack in the kiln.
  5. Firing. Kilns heat bricks to around 900–1,200 °C. The temperature and clay minerals decide the final colour, from pale yellow to deep blue-black.
  6. Cooling & sorting. Bricks cool gradually, then are graded and packed.

Famous Brick Buildings

Malbork Castle, Poland

Often described as the largest brick castle in the world, built by the Teutonic Knights.

Hampton Court Palace, England

Tudor red-brick grandeur with spectacular decorative chimneys.

Great Mosque of Djenné, Mali

The world's largest mud-brick building, re-plastered by the community every year.

Chilehaus, Hamburg

A ship-like 1920s office block and a landmark of Brick Expressionism.

St Pancras, London

A Victorian Gothic showpiece of red brick at the station's front.

Ctesiphon arch, Iraq

An ancient arch that remains among the largest single-span brick vaults ever built.

Care & Repointing Tips

General guidance only. For listed or structural work, consult a qualified professional. Curious how the brick you are repairing was made? Read how bricks are made.

New mortar FAQs: Types N, S, M and O, lime vs cement, how to mix mortar, building sand vs sharp sand, plus how to repoint brick, efflorescence, cleaning new brickwork, cold weather bricklaying plus new guides on sealing or painting brick, preblended mortar, salvaged brick and facing brick types FBX, FBS and FBA, and more in our trade guides.

Brick FAQ

What is the standard size of a brick?

It depends on the country. A UK metric brick is 215 × 102.5 × 65 mm, a US modular brick is 7⅝ × 3⅝ × 2¼ in, a German NF brick is 240 × 115 × 71 mm and a common Australian brick is 230 × 110 × 76 mm. Sizes are chosen so that, with a 10 mm mortar joint, one brick length equals two widths plus a joint.

What is the difference between English bond and Flemish bond?

English bond alternates whole courses of stretchers (long side showing) with whole courses of headers (end showing). Flemish bond alternates headers and stretchers within every course. Both are strong, traditional bonds; English bond is usually considered the stronger, Flemish bond the more decorative.

How are bricks made?

Clay or shale is dug, weathered, crushed and mixed with water, then shaped by extrusion and wire-cutting, by pressing into moulds, or by hand. The green bricks are dried slowly, fired in a kiln at around 900–1,200 °C, then cooled and sorted.

What mortar should I use to repoint an old brick wall?

Use a mortar that is softer and more permeable than the brick, so the joint takes the wear rather than the brick. On older buildings that usually means a lime mortar rather than a hard cement mortar.

Need quantities for a project? Try the brick calculator, or the mortar calculator for cement and sand per 1,000 bricks.

Take a Break: Mortar Smash

Our own original arcade game. Knock down the wall, one brick at a time.

Play now →